Posts: 412
Threads: 34
Joined: Mar 2017
Reputation:
7
Location: East of DFW
Oil? Same as any firearm that sits in waiting...
Posts: 25
Threads: 4
Joined: Jan 2016
Reputation:
0
I thought about oil or wax, just wasn't sure.
Sharkhide sounds like what I need. Thanks, Steve.
Dave, Thanks. Yes. I figured out what I wanted and had it made.
No machine shop here, just a drill press.
Rick
Posts: 1,156
Threads: 232
Joined: Jan 2016
Reputation:
20
Location: New Haven Ct
if you want to share the cool i'd be interested in a couple done.
very 1950's hot rod look to them.
Dave L.
Posts: 384
Threads: 27
Joined: Jan 2016
Reputation:
6
Location: Livermore, CA
07-05-2017, 11:27 AM
(This post was last modified: 07-05-2017, 11:40 AM by Jim Waltz.)
Sharkhide is cool stuff.
Clean metal and wipe it on.
http://www.sharkhide.com/
Interesting that the Cortec product was far superior to the "War on Rust" product.
Of course the testing was far more severe than most any circumstance we would experience in karting.
Jim Waltz, West Sacramento, CA